OEM Z308  Pure nickel cast iron electrode GB / T 10044 EZNi-1 AWS ENi-Cl JIS DFCNi Supplier, Factory

It is suitable for the welding of thin pieces of cast iron welding and machining surfaces, such as cylinder heads, important gray cast iron engine blocks, gear boxes, and Machine Tool and soon.

Product Description

🚀 APPLICATIONS
It is suitable for the welding of thin pieces of cast iron welding and machining surfaces, such as cylinder heads, important gray cast iron engine blocks, gear boxes, and Machine Tool and soon.
💎 CHARACTERISTICS
TQZ308 is pure nickel welding core, strong reduction of graphite type coating iron rod. It can be used in AC and DC dual purpose and is easy to operate. When welding, it is not necessary for weldment to preheat. It has good crack resistance and processability.
⚠️ PRECAUTIONS
  • Before welding, the electrodes need to be baked for 1 hour with the temperature of 150±10℃ before using.
  • It can eliminate welding stress and avoid crack by hammering the welding seam.
  • In order to reduce the impurity elements in the base metal penetration weld, narrow white band width, improve crack resistance and processing properties, it should use small current welding in cast iron cold welding.
📊 Chemical Composition of the deposited metal (%)
Elements C Si Mn S Fe Ni Other elements
Standard value ≤2.0 ≤2.5 ≤1.0 ≤0.03 ≤8.0 ≥90 ≤1.0
⚡ Welding Reference Current (AC, DC+)
Electrode diameter (mm) 2.5 3.2 4.0
Welding current (A) 60-90 90-110 120-150
🔧 Welding Distortion Correction

For deformation correction in hot state, mechanical correction and hammering are strictly prohibited in the range of blue brittle temperature (300℃~500℃) to avoid brittle cracks.

Flame Local Heating Requirements:

  • It is not advisable to repeat heating at the same part to avoid changes in the metallographic structure and mechanical properties.
  • Do not cause repeated corrections of tension and compression in the same part.
  • For hardenable welded parts, watering and rapid cooling are strictly prohibited.
  • Welding parts that need to be annealed should be rectified before annealing to eliminate internal stress.
  • The flame straightening heating temperature can be 700℃~850℃ (fuchsia), and should not exceed 900℃ (bright red) for low alloy structural steel.
❓ Frequently Asked Questions
What is TQZ308 welding electrode primarily used for?
It is ideal for welding thin cast iron pieces and machining surfaces, including cylinder heads, engine blocks, gear boxes, and machine tools.
Do I need to preheat the metal before using TQZ308?
No, when welding with TQZ308, it is not necessary for the weldment to be preheated, thanks to its excellent crack resistance.
What is the required baking procedure for these electrodes?
The electrodes should be baked for 1 hour at a temperature of 150±10℃ before they are used for welding.
How can I reduce welding stress during the process?
Welding stress can be eliminated and cracks avoided by hammering the welding seam after application.
What current should be used for a 3.2mm diameter electrode?
For a 3.2mm electrode, the recommended welding current range is 90-110 Amperes (AC or DC+).
What temperature range should be avoided for mechanical correction?
Mechanical correction and hammering are strictly prohibited within the blue brittle temperature range of 300℃ to 500℃ to prevent brittle cracks.