Used for welding high carbon steel, tool steel and dissimilar metals.
E312-16 is a duplex stainless steel electrode with a titanium-calcium coating. The welding process performance is excellent, suitable for both AC and DC. With approximately 40% ferrite content, it provides excellent crack resistance.
- Baking: Electrode shall be baked at 300-350℃ for 1 hour before use.
- Preparation: Remove rust, grease, moisture and other impurities before welding.
- Preheating: For hardenable steel or complex/thick workpieces, preheat at 150℃ when using small current.
Chemical Composition (Wt. %)
| Items | C | Mn | Si | S | P | Ni | Cr | Mo | Cu |
| Requirements | 0.15 | 0.5-2.5 | ≤1.0 | ≤0.03 | ≤0.04 | 8.0-10.5 | 28.0-32.0 | ≤0.75 | ≤0.75 |
| Typical Results | 0.09 | 1.08 | 0.76 | 0.010 | 0.028 | 9.97 | 29.0 | 0.12 | 0.17 |
| Items | Rm / MPa (Tensile Strength) | A / % (Elongation) |
| Requirements | ≥660 | ≥15 |
| Typical Results | 760 | 28 |
Typical Operating Procedures (AC or DC+)
| Diameter (mm) | 2.5 | 3.2 | 4.0 | 5.0 |
| Current (A) | 50-80 | 80-110 | 130-160 | 160-200 |
Packaging Details: 5kg/box, 4boxes/carton, 20kgs/carton, 50cartons/pallet. 21MT - 26MT per 1X20" FCL.
Material Compliance: Raw materials must comply with drawings and technical documents. Materials entering the factory are inspected according to GB/T 5117, GB/T 5118, and GB/T 8110 standards. Welding rods should not be baked more than twice and must be stored in an incubator after drying.
Frequently Asked Questions
What are the primary applications for E312-16 electrodes?
E312-16 is specifically designed for welding high carbon steel, tool steel, and joining dissimilar metals.
Does E312-16 work with AC or DC current?
Yes, it is versatile and provides excellent welding performance on both AC and DC (typically DC+) power sources.
Why does this electrode have high crack resistance?
The weld metal contains approximately 40% ferrite, which gives the duplex structure its superior resistance to cracking.
What is the required pre-welding preparation for the electrodes?
Electrodes must be baked at 300-350℃ for 1 hour before use to ensure moisture-free performance.
Are there specific instructions for welding thick or hardenable steel?
Yes, for hardenable steel or complex, thick workpieces, it is recommended to preheat the material to 150℃, especially when using lower current settings.
electrode,electrodes,welding,welding electrode,welding electrodes,welding rod,welding rods,welding electrode price,electrode welding,welding rod factory price,welding stick,stick welding,welding sticks,china welding rods,stick electrode,welding consumables,welding consumable,China electrode,welding electrodes China,carbon steel welding electrode,carbon steel welding electrodes,welding electrode factory,Chinese factory welding electrode,China welding electrode,China welding rod,welding rod price,welding supplies,wholesale welding supplies,global welding supplies,arc welding supplies,welding material supply,arc welding,steel welding,easy arc welding electrode,arc welding electrode,arc welding electrodes,vertical welding electrode,price of welding electrodes,cheap welding electrode,acid welding electrodes,alkaline welding electrode,cellulosic welding electrode,china welding electrodes,factory electrode,small size welding electrodes,welding materials,welding material,welding rod material,welding electrode holder,nickel welding rod,j38.12 e6013,welding rods e7018-1,welding stick electrode,welding rod 6010,welding electrode e6010,welding rod e7018,welding electrode e6011 ,welding rods e7018,welding electrodes 7018,welding electrodes e7018,welding rod 6013,welding rods 6013,welding electrode 6013,welding electrode e6013,6010 welding rod,6010 welding electrode,6011 welding rods,6011 welding electrodes,6013 welding rod,6013 welding rods,6013 welding electrode,6013 welding electrodes,7024 welding rod,7016 welding rod,7018 welding rod,7018 welding rods,7018 welding electrode,7018 welding electrodes,welding electrode e7016 ,e6010 welding rod,e6011 welding rod,e6013 welding rod,e7018 welding rod,e6013 welding electrode,e6013 welding electrodes,e7018 welding electrode,e7018 welding electrodes,J421 welding electrode,J422 welding electrodes,welding electrode J422,wholesale e6010,wholesale e6011,wholesale e6013,wholesale e7018,best welding electrode,best welding electrode J421,stainless steel welding electrode,stainless steel welding rod,stainless steel electrode,SS welding electrode,welding rods e307,welding electrode e312,309l welding rod,316 welding electrode,e316l 16 welding electrodes,cast iron welding electrode,aws Eni-Ci,aws Enife-Ci,surfacing welding,hard facing welding rod,hard surfacing welding,hardfacing welding, welding, welding,vautid welding,bohler welding,lco welding,miller welding, welding, welding,flux powder,welding flux,welding powder,welding electrode flux material ,welding electrode flux,welding electrode material,tungsten electrode,tungsten electrodes,welding wire,argon arc welding,mig welding,tig welding,gas arc welding,gas metal arc welding,electric are welding,electric arc welding,arc welding rods,carbon arc welding,e6013 welding rod uses,types of welding electrodes,flux core welding,types of electrodes in welding,welding supply,welding metal,metal welding,shielded metal arc welding,aluminum welding,welding aluminum with mig,aluminum mig welding,pipe welding,welding types,types of welding rod,all types of welding,welding rod types,6013 welding rod amperage,welding rods electrodes,welding electrode specification ,welding electrode classification ,welding electrode aluminium ,welding electrode diameter ,mild steel welding,stainless steel welding,e6011 welding rod uses,welding rods sizes,welding rods price,welding electrodes size,aws e6013,aws e7018,aws er70s-6,stainless steel welding wire,stainless steel mig welding wire,tig welding wire,low temp welding rod,6011 welding rod amperage,4043 welding rod,cast iron welding rod,western welding academy,sanrico welding rods,aluminium welding,aluminium welding rod,welding products,welding tech,welding factory